Thread: Honing question
View Single Post
Old 04-04-2013, 10:54 AM   #10 (permalink)
tjd10684
MCB Member
 
tjd10684's Avatar
 
Join Date: Jul 2009
Location: Beaver Falls PA (outside Pittsburgh)

Al03 is fine no need for boron

This honing process is technically a grinding process so i choose the material the same way I would for a standard grinding wheel. And your never supposed to grind a Al really without dressing the wheel frequently or you will load the load it up and destroy it. Same thing applies with honing but since you can't dress it you dunk it in oil and run it as little as possible knowing full well it WILL be ruined eventually. I do a quick hone on the raw sections of barrels when I bore them I only do it for like 10-15 sec just to take out the tool marks even then I only get about 100 barrels out of a hone before it's too loaded to work
__________________
My Feedback - http://www.mcarterbrown.com/forums/f...ml#post1575817

I also freak bore
http://www.mcarterbrown.com/forums/a...ml#post2393405

A wise man once said:
"The gap between theory and reality is not as far in theory as it is in reality."
tjd10684 is offline   Reply With Quote