One suggestion, the finish on the part going in the bath is the finish of it coming out so if it is uneven and pitted going in it will be uneven and pitted when you color it.

After you strip the parts either polish, blast or brush the parts to get them evened out.

Also make sure the parts are super clean before anodizing.

Lastly, as mentioned before do not let any ferrous material be in the ano bath as you noticed it will disolve and contaminate your bath.